Fluxite.
I would add a word of caution to Kevin (McMurdo) comments.
"modern" Fluxite contains zinc chloride, which will corrode away your joint and board very quickly. Washing with a solvent (IPA or whatever) does not remove any ZnCl/HCl occluded in the joint itself.
Look at the tin. The one I have warns clearly. See picture 2 below.
But I also have original pre 1960? tins, which is non- corrosive. I still use it, and if anyone wants a bit, send me a PM.
See my posting of 26 July 2017.
Three pictures. The first two are of the "modern" corrosive version, with the red devil. The third is the non-corrosive one, with a green devil, except that Kevin has a green devil on a presumably corrosive tin. Maybe, single colour printing on the tin is now preferred.
wme_bill
Attached Thumbnails
Click image for larger version

Name:	P1030181_fluxite 1R.jpg
Views:	127
Size:	62.7 KB
ID:	205983   Click image for larger version

Name:	P1030182_Fluxite 2R.jpg
Views:	130
Size:	61.7 KB
ID:	205984   Click image for larger version

Name:	P1030183_Fluxite 3R.jpg
Views:	130
Size:	57.2 KB
ID:	205985  
WME_bill is offline