Quote:
Originally Posted by kalee20 View Post
Quote:
Originally Posted by The Philpott View Post
The magical world of metallurgy- I still can't quite cope with Pb and Sn having medium melting points, and Pb/Sn alloys having a low melting point.
It's commonplace with any solution - table salt melts/solidifies at 801°C. Water/ice at 0°C. But brine (depending on concentration) may not freeze until -19°C, lower than either!
Ah, yes, but while there is a similarity between alloys and solutions, metallurgy and solution physics are not the same.

Colin.

Last edited by ColinTheAmpMan1; 7th Oct 2019 at 12:43 pm. Reason: more clarity.