Default Re: Discolouring of a GPO 746 phone?

I took my yellowed white Northern Electric 10 button 1554 and soaked it in some peroxide and warm water in the sunshine. Started around 10:00am and finishing up at 4:30. It wasn’t too bad considering the clouds covered the sun every now and then. Had it been sunny all day it would have taken less time.

Just soaked it in 1 part 20% peroxide and 4 parts warm water in the sunshine for about 6 1/2 hours. In this case 4 Gallons of warm water (15.12 L) to 1 Gallon 20% peroxide (3.78 L)

Make sure you wear rubber gloves when working with this mixture.
Attached Thumbnails
Click image for larger version

Name:	B-A.jpg
Views:	173
Size:	77.9 KB
ID:	183379   Click image for larger version

Name:	1 Before.jpg
Views:	142
Size:	86.3 KB
ID:	183380   Click image for larger version

Name:	2 Before.jpg
Views:	142
Size:	68.7 KB
ID:	183381   Click image for larger version

Name:	4.jpg
Views:	133
Size:	97.4 KB
ID:	183382   Click image for larger version

Name:	6 Dried.jpg
Views:	128
Size:	60.3 KB
ID:	183383  

DKD Contempra is offline